酒钢选矿厂选别工艺的改进与发展  被引量:7

Innovation and development of separation technology in Jiugang concentrator

在线阅读下载全文

作  者:王彩虹[1] WANG Caihong(Hongxing Iron&Steel Co.Lld.of Gansu Jiugang Group,Jiayuguan 735100,Gansu,Gansu)

机构地区:[1]甘肃酒钢集团宏兴钢铁股份有限公司,甘肃嘉峪关735100

出  处:《矿山机械》2022年第8期46-49,共4页Mining & Processing Equipment

摘  要:结合酒钢选矿厂桦树沟和黑沟两个矿区的难选氧化铁矿石性质,详细介绍了酒钢选矿厂从建厂至今,几次大的选别工艺变革、设备创新以及由此带来的选矿指标提升。矿石入选粒度由最初 15~100 mm 扩展到 0~100 mm,选别工艺由竖炉焙烧磁选发展到强磁选与焙烧磁选并存,再到焙烧磁选—浮选联合,最后发展为全粒级悬浮磁化焙烧—磁选—浮选联合新工艺,铁精矿品位由 47% 上升至 60%,回收率为 85%,精矿中 SiO含量由 11% 降至 5% 以下。Based on the nature of refractory iron oxide ore from Huashugou and Heigou mining zone of Jiugang concentrator,the paper in detail introduced several large innovations of separation technology and equipment reconstruction as well as sequent enhancement in separation indexes since the building of Jiugang concentrator.The feed size extended from original 15 ~ 100 mm to 0 ~ 100 mm,and the separation technology developed from shaft furnace roasting magnetic separation to the coexistence of high-intensity magnetic separation and roasting magnetic separation,and then to the combination of roasting magnetic separation and flotation,finally to the new combined process involving whole-sized suspension magnetic roasting,magnetic separation and flotation in sequence.The grade of iron concentrate increased from 47% to 60% with recovery ratio of 85%,SiOcontent in concentrate reduced from 11% to less than 5%.

关 键 词:铁矿石 选别工艺 竖炉焙烧 悬浮磁化焙烧 强磁选 

分 类 号:TD92[矿业工程—选矿]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象