航空子午线轮胎胎侧胶配方的优化设计  

Optimum Design of Sidewall Compound Formula of Aviation Radial Tire

在线阅读下载全文

作  者:吴洪全 黄义钢 常爱修 臧云红 WU Hongquan;HUANG Yigang;CHANG Aixiu;ZANG Yunhong(Qingdao Doublestar Tire Industry Co.,Ltd,Qingdao 266400,China)

机构地区:[1]青岛双星轮胎工业有限公司,山东青岛266400

出  处:《轮胎工业》2023年第3期172-176,共5页Tire Industry

摘  要:对航空子午线轮胎胎侧胶配方进行优化设计。试验结果表明:胎侧胶优选配方为天然橡胶65,顺丁橡胶35,炭黑N37550,增粘树脂Koresin 2,防老剂5.5,不溶性硫黄1.8,促进剂TBBS 0.8,其他8.7;与生产配方胶料相比,试验配方胶料的门尼焦烧时间延长,加工安全性和抗硫化返原性能提高,硫化胶的密度减小,拉伸强度、拉断伸长率和撕裂强度增大,耐低温和耐屈挠性能提高;成品轮胎的导电性能达到相关标准要求。The sidewall compound formula of aviation radial tires was optimized.The test results showed that the optimum formula of sidewall compound was:natural rubber 65,cis-polybutadiene rubber 35,carbon black N37550,tackifying resin Koresin 2,antioxidant 5.5,insoluble sulfur 1.8,accelerator TBBS 0.8 and others 8.7.Compared with the production formula compound,the Mooney scorch time of the test formula compound was prolonged,the processing safety and anti-reversion properties were improved.Moreover,the density of the vulcanizate was reduced,the tensile strength,elongation at break and tear strength increased,and the low temperature resistance and flexural resistance were improved.Additionally,the electrical conductivity of the finished tire met the requirements of relevant standards.

关 键 词:航空子午线轮胎 胎侧胶 物理性能 耐低温性能 耐屈挠性能 导电性能 

分 类 号:U463.341.6[机械工程—车辆工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象