Countermeasures for Forming Defects of Ultra-thin Glass Producing on Wide Rolling Line

在线阅读下载全文

作  者:李文 LI Wen(Caihong(Yan'an)New Energy Company Limited,Yan'an 716000,China)

机构地区:[1]彩虹(延安)新能源有限公司,延安716000

出  处:《玻璃》2023年第9期47-51,共5页Glass

摘  要:宽体压延线超薄玻璃成形作业难度大,对装备、工具、方法等方面都有较高的要求。通过分析研究找出宽体压延线超薄玻璃的成形缺陷原因,对厚薄差大、热粘、亮斑、辊伤、波形不良等缺陷提出对策建议,稳定成形工艺,提高产品良率。Ultra-thin glass forming operation on wide rolling line is difficult,the demands on equipment,tools,methods is stricter.Through analysis and research,the causes of forming defects of ultra-thin glass on wide rolling line are found out.The countermeasures and suggestions on the defects such as large thickness difference,hot sticking,bright spot,roll damage and poor waveform are put forward,so as to stabilize the forming process and increase the product yield.

关 键 词:宽体压延线 超薄玻璃 作业难度 缺陷 对策 

分 类 号:TQ171[化学工程—玻璃工业]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象