纳米粘土在半钢子午线轮胎胎侧胶中的应用  被引量:1

Application of Nano-clay in Sidewall Compound of Steel-belted Radial Tire

在线阅读下载全文

作  者:吉雷波 张华涛 曹伟 华振 孙华 JI Leibo;ZHANG Huatao;CAO Wei;HUA Zhen;SUN Hua(Zaozhuang Sanxing Advanced Materials Co.,Ltd,Zaozhuang 277319,China;Shandong Dagong Rubber Co.,Ltd,Zaozhuang 277100,China)

机构地区:[1]枣庄市三兴高新材料有限公司,山东枣庄277319 [2]山东大工橡胶股份有限公司,山东枣庄277100

出  处:《轮胎工业》2023年第9期545-548,共4页Tire Industry

摘  要:研究纳米粘土在半钢子午线轮胎胎侧胶中的应用。结果表明:以一定量的纳米粘土替代炭黑N660,胶料的加工性能和硫化特性变化不大,硫化胶的拉断伸长率和撕裂强度明显增大;随着纳米粘土用量的增大,硫化胶的密度增大,定伸应力减小,耐屈挠疲劳性能提高;以纳米粘土等量替代炭黑N660,填料分散性稍好,成品轮胎的高速和耐久性能达到企业标准要求,胶料成本下降。The application of nano-clay in the sidewall compound of steel-belted radial tires was studied.The results showed that by using a certain amount of nano-clay to replace the same amount of carbon black N660,the elongation at break and tear strength of the vulcanizate increased significantly,while the processability and vulcanization characteristics of the compound changed little.As the dosage of nano-clay increased,the density of the vulcanizate increased,the modulus decreased,and the flexural fatigue resistance was improved.In addition,the filler dispersion was slightly improved,the high speed performance and durability of the finished tire met the requirements of the enterprise standards,and the compound cost was reduced.

关 键 词:纳米粘土 半钢子午线轮胎 胎侧胶 耐屈挠疲劳性能 成本 

分 类 号:TQ330.383[化学工程—橡胶工业]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象