摘 要:在加压湿法冶炼过程中,通过降低正常排气阀门的开度或提高反应温度,可提高氧气利用率。不同的物料,氧气利用率也存在差异,钴铜硫化矿的氧气利用率最高,可达82%~87%;赤铁矿法除铁生产的氧气利用率最低,但加强生产控制也可以提高氧气利用率。In the process of pressurized wet smelting,oxygen utilization can be improved by reducing the opening of normal exhaust valves or increasing reaction temperature.There are also differences in oxygen utilization rates among different materials.Cobalt copper sulfide ore has the highest oxygen utilization rate,up to 82%~87%,and the oxygen utilization rate produced by hematite method for iron removal is the lowest.Strengthening production control can also improve oxygen utilization efficiency.
分 类 号:TF831[冶金工程—有色金属冶金]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.43