作 者:徐文静 梁建荣 曲萌菲 王艺璇 侯冰娜 赵琳琳[2] 张杭 李征征 XU Wenjing;LIANG Jianrong;QU Mengfei;WANG Yixuan;HOU Bingna;ZHAO Linlin;ZHANG Hang;LI Zhengzheng(School of Chemical Engineering and Materials,Tianjin University of Science and Technology,Tianjin 300457,China;School of Materials Science and Engineering,Tianjin University of Technology,Tianjin 300457,China;State Key Laboratory of Molecular Engineering of Polymers,Fudan University,Shanghai 200433,China)
机构地区:[1]天津科技大学化工与材料学院,天津300457 [2]天津理工大学材料科学与工程学院,天津300457 [3]复旦大学聚合物分子工程国家重点实验室,上海200433
出 处:《材料工程》2023年第11期144-150,共7页Journal of Materials Engineering
基 金:天津市教委科研计划项目(2018KJ110)。
摘 要:合成一种基于动态亚胺键的自愈合氧化海藻酸钠-乙二醇壳聚糖水凝胶(OSA-GC),将海藻酸钠通过高碘酸钠氧化合成氧化海藻酸钠(OSA),并与乙二醇壳聚糖(GC)发生席夫碱反应制备具有不同交联度的自愈合OSA-GC水凝胶,研究GC的浓度对OSA-GC水凝胶的微观形态、黏弹性能、溶胀性能、自愈合性能、降解速率和体外药物释放性能的影响。结果表明:OSA-GC水凝胶具有多孔结构,通过控制OSA与GC的质量比,OSA-GC水凝胶的孔径处于50~280μm;OSA-GC水凝胶的溶胀率在120 h达到溶胀平衡,溶胀率达到71.3~112.1。OSA-GC水凝胶在含有溶菌酶(10 mg/mL)的PBS中发生降解,在12天后OSA-GC水凝胶的质量损失达到43.1%~51.9%;在室温条件下,OSA-GC水凝胶在无外界刺激时2 h实现自愈合,负载吉西他滨的OSA-GC自愈合水凝胶对抗癌药物吉西他滨具有缓释作用,药物释放时间可达48 h,药物释放量达到72.6%~89.5%。OSA-GC自愈合水凝胶在药物载体领域具有较好的应用前景。The self-healing oxidized sodium alginate-glycol chitosan hydrogel(OSA-GC)based on dynamic imine bonds was synthesized.Oxidized sodium alginate(OSA)was synthesized by oxidizing sodium alginate with sodium periodate,and self-healing OSA-GC hydrogels with different cross-linking degrees were prepared by Schiff base reaction with glycol chitosan(GC).The effect of GC concentration on the microscopic morphology,viscoelasticity,swelling performance,self-repair performance,degradation rate and in vitro drug release performance of OSA-GC hydrogels were investigated.The results show that OSA-GC hydrogels have the characteristics of porous structure with a pore size ranging from 50μm to 280μm by controlling the mass ratio of OSA to GC.The OSA-GC hydrogels can reach the swelling equilibrium at 120 hours,and the swelling ratio reach 71.3-112.1.OSA-GC hydrogel can be degraded in PBS containing lysozyme(10 mg/mL),and the mass loss of OSA-GC hydrogel is 43.1%-51.9% after 12 days.At room temperature,OSA-GC hydrogels can achieve self-healing within 2 h in the absence of external stimuli.OSA-GC hydrogel loaded with gemcitabine shows a sustained release effect on the anticancer drug gemcitabine,and the release time can reach 48 hours in the drug release experiment,which shows promising application prospects in biomedical fields of drug carriers.
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.222