高岭土伴生型石英分粒级制备光伏玻璃用石英砂  被引量:1

Preparation of Quartz Sand for Solar Photovoltaic Glass from Quartz Associated Kaolin by Size Fraction Distribution

在线阅读下载全文

作  者:张乾伟 吴建新 方强 刘小康 杜润生 孙凤军 Zhang Qianwei;Wu Jianxin;Fang Qiang;Liu Xiaokang;Du Runsheng;Sun Fengjun(CNBM Research Institute for Advanced Glass Materials Group Co.,Ltd,Bengbu,Anhui,China;State Key Laboratory for Advanced Technology of Float Glass,Mineral&Resources Institute,Bengbu,Anhui,China;Lanling County Yixin Mining Technology Co.,Ltd.Linyi,Shandong,China)

机构地区:[1]中建材玻璃新材料研究院集团有限公司,安徽蚌埠233000 [2]浮法玻璃新技术国家重点实验室矿产资源研究所,安徽蚌埠233000 [3]兰陵县益新矿业科技有限公司,山东临沂277713

出  处:《矿产综合利用》2023年第6期9-14,共6页Multipurpose Utilization of Mineral Resources

基  金:安徽省重点研发计划(202104a05020034);安徽省科技重大专项(201903a05020002);山东省重大科技创新工程(2019JZZY010317)。

摘  要:这是一篇陶瓷及复合材料领域的论文。为助力碳中和、碳达峰目标,我国光伏玻璃需求量近年来快速增长,从而使光伏玻璃用低铁石英砂(ωFe_(2)O_(3)≤0.010%)供应趋紧,因此高岭土伴生型石英制备低铁石英砂备受关注。高岭土伴生型石英通常可在高岭土物理选矿的尾矿中富集,以广西合浦某高岭土物理选矿尾矿为实验对象,研究了分粒级选矿提纯对高岭土伴生型石英制备低铁石英砂的影响规律。结果表明,高岭土伴生型石英矿中+2mm粒级的SiO_(2)、Al_(2)O_(3)、Fe_(2)O_(3)含量优于0.71~2mm、0.125~0.71mm粒级相应指标;采用磨矿-分级-磁选-浮选的分粒级选矿提纯工艺,不同粒级所得浮选石英精砂的Fe_(2)O_(3)含量均不低于0.016%;对+2 mm粒级浮选精砂分别采用硫酸、草酸与氢氟酸、草酸为酸浸介质所得石英精砂的Fe_(2)O_(3)含量分别降至0.0091%、0.0054%,满足光伏玻璃、光学玻璃用低铁石英砂的Fe_(2)O_(3)含量要求。This is an essay in the field of ceramics and composites.To achieve carbon neutrality and peaking carbon dioxide emissions,the low-iron quartz sand(ωFe_(2)O_(3)≤0.010%)supply for photovoltaic glass is tightening in China,so the preparation of low-iron quartz sand from quartz associated with kaolin gradually attracting widespread attention.However,quartz associated with kaolin can usually be enriched in the tailings of kaolin physical beneficiation.Taking quartz associated kaolin which is from tailings of kaolin physical beneficiation in Hepu,Guangxi as the object,the effect of purification by size fraction distribution on the preparation of low iron quartz sand from quartz-associated kaolin was studied in this essay.The experimental results showed that the index of SiO_(2),Al_(2)O_(3)and Fe_(2)O_(3)content in size of 2 mm or more was better than that of 0.71~2 mm and 0.125~0.71 mm respectively,but for all different size fraction products,ferric oxide content of quartz sand is not less than 0.016%by grinding,hydraulic classification,magnetic separation and flotation.The content of quartz sand obtained by sulfuric acid and oxalic acid was 0.0091%,and the content of quartz sand obtained by hydrofluoric acid and oxalic acid was 0.0054%respectively,both of which meets the ferric oxide content requirement of low iron quartz sand for solar photovoltaic glass and optical glass.

关 键 词:陶瓷及复合材料 高岭土 石英 分粒级 提纯 

分 类 号:TD97[矿业工程—选矿]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象