磷矿中磷灰石及脉石与盐酸反应活性的研究  

Study on Reactivity of Apatite and Gangue in Phosphate Rock with Hydrochloric Acid

在线阅读下载全文

作  者:方进 覃艳 孟品品 冷为贵 周骏宏[3] 张凌云 黄德明 陈彪 袁光富 李青青 李忠艳 黄仕英 FANG Jin;QIN Yan;MENG Pinpin;LENG Weigui;ZHOU Junhong;ZHANG Lingyun;HUANG Deming;CHEN Biao;YUAN Guangfu;LI Qingqing;LI Zhongyan;HUANG Shiying(Guizhou Batian Ecological Engineering Co.,Ltd.,Weng′an,Guizhou 550400,China;Phosphorus Sulfur Titanium Resource Comprehensive Utilization Engineering Research Center,Weng′an,Guizhou 550400,China;Phosphorus Chemical Laboratory of Qiannan Normal University for Nationalities,Duyun,Guizhou 558000,China;Shenzhen Batian Ecological Engineering Co.,Ltd.,Shenzhen,Guangdong 518000,China;Guangxi Plant Nutrition Engineering Technology Research Center,Guigang,Guangxi 537100,China)

机构地区:[1]贵州芭田生态工程有限公司,贵州瓮安550400 [2]磷-硫-钛资源综合利用工程研究中心,贵州瓮安550400 [3]黔南民族师范学院磷化工实验室,贵州都匀558000 [4]深圳市芭田生态工程股份有限公司,广东深圳518000 [5]广西植物营养工程技术研究中心,广西贵港537100

出  处:《肥料与健康》2024年第1期62-67,共6页Fertilizer & Health

基  金:贵州省科技计划项目(黔科合成果[2022]一般088);贵州省科技计划项目(黔科中引地[2021]4014);贵州省科技计划项目(黔科合支撑[2021]一般307);大学生创新创业项目(202210670055)。

摘  要:选用主要组分为磷灰石、石英、白云石的中低品位磷矿与盐酸溶液进行反应,考察了反应后的残渣质量、残渣中P2O5的含量以及残渣的X射线衍射图谱等。结果表明:原料磷矿与5%(体积分数,下同)盐酸溶液反应30 min后,白云石相基本消失,残渣中P2O5的质量分数由27.81%升至29.40%;采用10%的盐酸溶液,磷灰石开始参与反应;采用25%的盐酸溶液反应30 min后,残渣中P2O5的质量分数降至0.13%,磷灰石相基本消失。通过控制盐酸溶液体积分数,可选择性地使原料磷矿中的组分与盐酸溶液反应,达到酸法选矿、避免产生磷尾矿的目的。Middle and low grade phosphate rock,which are composed of apatite,quartz and dolomite mainly,is selected to react with hydrochloric acid solution.The residue weight,the content of P 2O 5 in residue and the X-ray diffraction pattern of the residue after the reaction are investigated.The results show that after reacting with 5%(volume fraction,the same below)hydrochloric acid solution for 30 minutes,the dolomite phase has almost disappeared,and the mass fraction of P 2O 5 in the residue increases from 27.81%to 29.40%;with 10%hydrochloric acid solution,apatite begins to participate in the reaction;after reacting with 25%hydrochloric acid solution for 30 minutes,the mass fraction of P 2O 5 in the residue decreases to 0.13%,and the apatite phase has almost disappeared.Therefore,by controlling the volume fraction of hydrochloric acid solution,the components of raw phosphate rock can be selectively reacted with hydrochloric acid solution,so as to achieve the purpose of acid beneficiation and avoid the production of phosphate tailings.

关 键 词:磷矿 化学选矿 中低品位 磷灰石 脉石 盐酸 尾矿 

分 类 号:TD97[矿业工程—选矿]

 