厄瓜多尔某铜尾矿浆絮凝沉降优选絮凝剂试验  

Test on Priority Selection Flocculant of Flocculation and Sedimentation of Copper Tailings Slurry in Ecuador

在线阅读下载全文

作  者:岳守艳 庞增瑞 YUE Shouyan;PANG Zengrui(BGRIMM Technology Group;BGRIMM Chemical Technology(Cangzhou)Co.,Ltd.)

机构地区:[1]矿冶科技集团有限公司,北京市大兴区102628 [2]北矿化学科技(沧州)有限公司

出  处:《现代矿业》2024年第2期239-242,共4页Modern Mining

摘  要:为提高厄瓜多尔某铜矿浓密机的处理效率,降低输送成本,减少跑浑现象,进行了尾矿絮凝沉降试验。结果表明:矿浆浓度16.67%、絮凝剂用量20 g/t时,添加絮凝剂BK816F,尾矿浆沉降速度最快,沉降80 s后清水层高度即可达15 cm;矿浆浓度30%时,随着絮凝剂添加量的增大,尾矿浆沉降速度总体加快,其中BK816F效果最明显,可在较低用量、较短时间内达到较好的沉降效果;质量浓度同为0.1%的絮凝剂溶液,BK816F的黏度最低。各项性能指标均表明,BK816F可作为该铜矿的高效絮凝剂。In order to improve the treatment efficiency of thickener in a copper mine of Ecuador,re-duce the transportation cost and reduce the phenomenon of muddy running,the flocculation sedimentation test of tailings was carried out.The results show that when the slurry concentration is 16.67%,the flocculant dosage is 20 g/t,and the flocculant BK816F is added,the sedimentation rate of the tailings slurry is the fast-est,and the height of the clear water layer can reach 15 cm after 80 s of sedimentation.When the slurry con-centration is 30%,the sedimentation rate of tailings slurry is generally accelerated with the increase of floc-culant dosage,and the effect of BK816F is the most obvious,which can achieve better sedimentation effect in a lower dosage and a shorter time.The viscosity of BK816F is the lowest when the mass concentration of flocculant solution is all 0.1%.All the performance indexes show that BK816F can be used as an efficient flocculant for the copper mine.

关 键 词:铜尾矿 浓缩脱水 沉降试验 高效絮凝剂 

分 类 号:TD926.4[矿业工程—选矿]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象