焊缝跟踪孔洞尺寸对锌锅气刀条纹的影响及其优化  

The Influence and Optimization of Weld Tracking Hole Size on Air Knife Streaks after Passing through the Zinc Pot

在线阅读下载全文

作  者:余振华 Yu Zhenhua(Cold Rolling Mill of Wuhan Iron and Steel Co.Ltd.,Wuhan 430080,Hubei)

机构地区:[1]武汉钢铁有限公司冷轧厂,湖北武汉430080

出  处:《武汉工程职业技术学院学报》2024年第1期21-23,共3页Journal of Wuhan Engineering Institute

摘  要:在连续热镀铝锌机组,因锌锅中锌液的铝含量较高,锌液黏度低,当带钢焊缝区域通过锌锅气刀后,会产生气刀条纹。介绍了焊缝区域过锌锅气刀后,带钢表面气刀条纹产生的原因,并通过计算优化了焊机冲孔冲头尺寸,减少了焊缝区域过气刀后气刀条纹产生的概率。In continuous hot aluminum-zinc plating line,due to the high aluminum content of zinc liquid in and low viscosity of zinc liquid,the air knife streaks appear when the weld of the steel pass through zinc pot.This paper introduces the causes of the air knife streaks of the strip surface through the welding,and optimizes the size of the punch of the welder through calculation,thus reducing the probability of air knife streaks when the welding go through the air knife.

关 键 词:气刀条纹 孔洞 气流 热镀锌 表面质量 

分 类 号:TG332[金属学及工艺—金属压力加工]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象