作 者:刘敏敏 王振宇 刘昊[3] 张宁 LIU Minmin;WANG Zhenyu;LIU Hao;ZHANG Ning(Beijing Institute of Residential Building Design&Research Co.,Ltd.,Beijing 100005,China;Faculty of Architecture,Civil and Transportation Engineering,Beijing University of Technology,Beijing 100124,China;Beijing Yugu Co.,Ltd.,Beijing 100070,China)
机构地区:[1]北京市住宅建筑设计研究院有限公司,北京100005 [2]北京工业大学城市建设学部,北京100124 [3]北京榆构有限公司,北京100070
出 处:《建筑结构》2024年第10期8-13,117,共7页Building Structure
基 金:北京市东城区优秀人才培养资助项目(2021-dchrcpyzz-51)。
摘 要:提出一种用于装配式剪力墙结构的螺栓连接的干式连接方法,即预制墙板上预埋钢件,上、下层墙体通过高强螺栓和预埋钢件进行连接。为研究高强螺栓连接装配式混凝土剪力墙的抗震性能,对1个现浇试件和2个高强螺栓连接试件进行拟静力试验,对试件的破坏特征、滞回性能、变形能力、承载能力、耗能能力及延性等进行分析。结果表明:高强螺栓连接装配式剪力墙有效实现了剪力墙构件的工作机制,滞回曲线饱满,耗能能力较强,抗震性能良好。现浇试件RCSW、钢筋焊接试件DCSW1、钢筋环绕型试件DCSW2的极限位移角分别达到了1/60、1/60和1/41;钢筋焊接试件DCSW1的裂缝开展形态、受力性能及破坏形态与现浇试件RCSW相似,耗能曲线基本一致,耗能能力接近;钢筋环绕型试件DCSW2的屈服荷载、峰值荷载和极限荷载均小于RCSW和DCSW1,墙体塑性变形偏小,耗能能力偏低。A dry connection method for bolt connection of prefabricated concrete shear wall structure was proposed,embedded steel parts in prefabricated wall panels,the upper and lower walls are connected by high-strength bolts and embedded steel parts.In order to study the seismic performance of prefabricated concrete shear walls connected by high-strength bolts,a pseudo-static test was carried out on a cast-in-place specimen and two high-strength bolt connection test specimen,the failure characteristics,hysteresis performance,deformation capacity,bearing capacity,energy dissipation capacity and ductility of the specimen were analyzed.The result shows that high-strength bolt connection fabricated shear wall effectively realizes the working mechanism of shear wall components,it has full hysteresis curve,strong energy consumption and good seismic performance.The ultimate displacements of the cast-in-place specimen RCSW、the steel bar welding specimen DCSW1、the steel-encircled specimen DCSW2 reached 1/60,1/60 and 1/41.The crack development pattern,stress performance and failure pattern of the steel bar welding specimen DCSW1 are similar to those of the cast-in-place specimen RCSW,the energy consumption curve is basically the same,and the energy consumption capacity is close;The yield load,peak load and ultimate load of the steel-encircled specimen DCSW2 are all smaller than RCSW and DCSW1,the wall plastic deformation is relatively small,and the energy dissipation capacity is relatively low.
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.7