氯离子对不锈钢冷却水管道腐蚀的分析及研究  

Analysis and Research on the Corrosion of Stainless Steel Cooling Water Pipe Caused by Chloride Ions

在线阅读下载全文

作  者:李辉 姚月姣[2] LI Hui;YAO Yue-jiao(Automotive Engineering Corporation,Tianjin 300113,China;CCCC First Harbor Consultants Co.Ltd.,Tianjin 300222,China)

机构地区:[1]中国汽车工业工程有限公司,天津300113 [2]中交第一航务工程勘察设计院有限公司,天津300222

出  处:《工程建设与设计》2024年第13期65-67,共3页Construction & Design for Engineering

摘  要:我国北方某已建项目中,不锈钢冷却水管道上出现多处孔蚀缺陷,论文以此为案例展开研究,分析不锈钢腐蚀的机理,研究不锈钢腐蚀的影响因素,提出适用于同类项目的氯离子浓度限值和相应的防腐解决方案,如改进焊接工艺、投加化学药剂、优化补水水质、保持系统的定期运行等。In a project that has been built in north China,there are multiple cavitation defects on stainless steel cooling water pipes.This paper takes this as a case study to analyze the mechanism of stainless steel corrosion,study the influencing factors of stainless steel corrosion,and propose chloride ion concentration limits applicable to similar projects and corresponding anti-corrosion solutions,such as improving the welding process,adding chemical agents,optimizing the water quality of the water supply,and maintaining the regular operation of the system.

关 键 词:工业冷却循环水 不锈钢管道 氯离子 腐蚀 浓度限值 

分 类 号:TQ050.9[化学工程]

 