作  者:王莉莉[1,2] 胡芳问 付世博 王鑫 付海朋[1,2] 吴健辉 李栋 石健[4] WANG Lili;HU Fangwen;FU Shibo;WANG Xin;FU Haipeng;WU Jianhui;LI Dong;SHI Jian(School of Architecture and Civil Engineering,Northeast Petroleum University,Daqing 163318,Heilongjiang China;Heilongjiang Provincial Key Laboratory of Thermal Utilization and Disaster Reduction of New Energy in Cold Regions,Daqing 163318,Heilongjiang China;Natural Resources and Construction Management Bureau of Daqing High-tech Industrial Development Zone,Daqing 163318,Heilongjiang China;Water Supply and Drainage Room,Institute of Process Research,Ninth Oil Production Plant,Daqing Oilfield,Daqing 163853,Heilongjiang China)

机构地区:[1]东北石油大学土木建筑工程学院,黑龙江大庆163318 [2]黑龙江省寒区新能源热利用及防灾减灾重点实验室,黑龙江大庆163318 [3]大庆高新技术产业开发区自然资源与建设管理局,黑龙江大庆163318 [4]大庆油田第九采油厂工艺研究所给水排水室,黑龙江大庆163853

出  处:《河南科学》2024年第8期1111-1119,共9页Henan Science

基  金:大庆油田有限公司委托技术开发项目(DQYT-0509003-2023-JS-761)。

摘  要:CCUS-EOR系统中的转油站掺水回注系统管线极易受回注污水腐蚀影响而发生腐蚀泄漏风险.针对此问题,基于流体力学、电化学腐蚀原理建立了稳态非等温流动模型和腐蚀电化学模型,开展管线CO_(2)流动和腐蚀电化学特性研究,分析流速、温度、压力和pH值等因素对管线腐蚀状态的影响.研究结果表明,直管和弯管局部区域存在流速增加现象,弯管处易发生空蚀破坏;管内回注污水流速越快,pH值越低,温度越高,管线管径越小,管道内壁的腐蚀速率越高.管线设计建议优选非金属管道,若采用碳钢金属管道,工程设计上应尽量选择较大管径的管材,同时可考虑添加缓蚀剂以调节pH值,降低污水输送的温度,从而降低管道内壁的腐蚀速率.In CCUS-EOR systems,the water injection system at the transfer station is highly susceptible to corrosion and leakage due to the corrosive impact of reinjected wastewater.To address this issue,a steady-state non-isothermal flow model and an electrochemical corrosion model were developed based on fluid dynamics and electrochemical principles.The study investigated the flow and electrochemical corrosion characteristics of CO_(2) within the pipeline,analyzing factors such as flow velocity,temperature,pressure,and pH on pipeline corrosion.The results revealed increased flow velocity in specific areas of both straight and curved sections,with cavitation damage prone to occurring in curved sections.Faster flow rates of reinjected wastewater,lower pH values,higher temperatures,and smaller pipeline diameters were associated with higher corrosion rates on the inner walls of the pipeline.Non-metallic pipelines are recommended for pipeline design.If carbon steel pipelines are chosen,the design should prioritize larger diameters.Additionally,adding corrosion inhibitors to adjust pH values and lowering the temperature of wastewater transport can reduce the corrosion rate on the inner walls of the pipeline.

关 键 词:CCUS-EOR 非等温流动 电化学腐蚀 数值模拟 掺水回注管线 

分 类 号:TE988.2[石油与天然气工程—石油机械设备]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象