LF精炼无氟渣系生产Q345qE钢的实践  

Procduction Practice of Q345qE Steel with Fluorine-free Slag System in LF Refining

在线阅读下载全文

作  者:栾文林[1] 刘志远[1] 王重君 么敬文 孔明姣 Luan Wenlin;Liu Zhiyuan;Wang Chongjun;Yao Jingwen;Kong Mingjiao(Tangshan Meium and Heavy Plate Co.,Ltd.)

机构地区:[1]唐山中厚板材有限公司

出  处:《宽厚板》2024年第3期24-26,共3页Wide and Heavy Plate

摘  要:根据不同精炼渣系的特点,选择无氟的CaO-Al_(2)O_(3)-SiO_(2)渣系,确定了含铝钢精炼终渣最佳组成为w(CaO)51%~54%、w(SiO_(2))4%~7%、w(Al_(2)O_(3))28%~31%。优化转炉脱氧工艺,在转炉出钢过程中进行顶渣控制,取得目标渣系。采用循环渣利用技术,取消了在精炼工序加入萤石的操作。生产实践表明:无氟渣系满足了BOF-LF-CC工艺生产Q345qE钢的要求,为高效、清洁生产奠定了基础。Based on the characteristics of different refining slag systems,a fluorine-free CaO-Al_(2)O_(3)-SiO_(2) slag system is selected,and the optimal chemcial composition of the refining final slag for aluminum containing steel is determined,i.e.,w(CaO)of 51%~54%,w(SiO_(2))of 4%~7%,and w(Al_(2)O_(3))of 28%~31%.The deoxidation process of the converter is optimized,and the top slag control is implemented during the converter steelmaking to obtain the target slag system.The slag recycling technique is applied,the fluorite addition operation during refining is cancelled.The production practice shows that the fluorine-free slag system satisfies the requirements of Q345qE steel production by BOF-LF-CC process,which lays the solid foundation for efficient and clean production.

关 键 词:LF 无氟精炼渣 脱氧 脱硫 

分 类 号:TF769.2[冶金工程—钢铁冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象