检索规则说明:AND代表“并且”;OR代表“或者”;NOT代表“不包含”;(注意必须大写,运算符两边需空一格)
检 索 范 例 :范例一: (K=图书馆学 OR K=情报学) AND A=范并思 范例二:J=计算机应用与软件 AND (U=C++ OR U=Basic) NOT M=Visual
作 者:Aleksandr V.Stankevich Nikolay A.Rasputin Anisa KhRudina Gennady L.Rusinov Vera I.Filyakova Valery N.Charushin
机构地区:[1]I.Ya. Postovsky Institute of Organic Synthesis, Ural Branch of the Russian Academy of Sciences,ekaterinburg 620108,russia [2]Russian Federal Nuclear Center-Zababakhin All-Russia Research Institute of Technical Physics,snezhinsk 456770,russia [3]Kazan National Research Technological University,kazan 420015,russia
出 处:《Defence Technology(防务技术)》2024年第10期210-224,共15页Defence Technology
基 金:supported by the Ministry of Science and Higher Education of the Russian Federation(Agreement with Zelinsky Institute of Organic Chemistry RAS Grant No.075-15-2020-803).
摘 要:In this work, comprehensive studies of 2,4-dinitroanisole(2,4DNAN) were carried out using powder thermorentgenography of the internal standard. The time of the complete polymorphic transition in the solid phase β→a in 2,4DNAN under various combinations of conditions has been determined. It has been established that, regardless of the season of manufacture of the substance, when it is stored for 8-9months, with a change in ambient temperature from minus 30℃ to plus 30℃, a complete polymorphic transition β→a occurs. When stored in conditions below minus 5℃, polymorphic transition does not occur. When stored in conditions above plus 30℃ in a closed container, polymorphic transition occurs within 3 weeks. The polymorphic transition is accompanied by a decrease in density by 1.3%-1.5% and an increase in melting temperature by 10-12℃, depending on the degree of purity of the starting substance. The activation energy of the molecular rearrangement was 68-70 k J/mol(16.5 ± 3 kcal/mol). The mechanism of polymorphic transition has been evaluated, which is presumably based on internal homodiffusion and energy transfer to the surface of the mass of powder particles and the product. The average activation energy of the polymorphic transition process was 110 ± 6.2 k J/mol(26.2 kcal/mol). In an open container, reactions proceed by a homogeneous mechanism, and in a closed container by a heterogeneous mechanism involving the gas phase.
关 键 词:Energetic materials Melt-castable 2 4-Dinitroanisole Polymorphic transition Kinetics Mechanism Homodiffusion SUBLIMATION