作 者:Mingyang Wang Yuanyuan Ji Da-Hai Xia Dejing Zhou Yesen Zhu Zhiming Gao Zhenbo Qin Wenbin Hu
机构地区:[1]School of Materials Science and Engineering,Tianjin University,Tianjin 300350,China [2]Yin Bang Clad Mat Co Ltd,Jiangsu Key Lab Clad Mat,Wuxi 214145,China [3]PowerChina Huadong Engineering Corporation Limited,Hangzhou 311122,China
出 处:《Journal of Materials Science & Technology》2024年第9期57-68,共12页材料科学技术(英文版)
基 金:financed by the National Key Research and Development Program(No.2022YFB3705801);the National Natural Science Foundation of China(Nos.52031007 and 52171077).
摘 要:Electrochemical and localized corrosion behavior of a 4045/7072/3003 M/4045 Al alloy composite in 3.5 wt.%NaCl solution was investigated from cross-sectional and plane directions by electrochemical impedance spectroscopy,polarization curves,and high-resolution microscopic examination.Plane directions showed higher corrosion resistance than the cross-sectional surface,with almost all localized corrosion initiated from Si-containing inclusions.The cross-section showed a complex galvanic effect among the four layers,the galvanic coupling between 4045/7072 accelerated the dissolution of 7072 because 7072 served as the anode,however,the galvanic coupling between 3003 M/4045 protected 4045 from corrosion,indicating that 3003 M served as the anode.
关 键 词:Al alloy composite sheet Localized corrosion Electrochemical behavior