浮法锡槽槽底泡的研究与解决方案  

Research and Solutions for Bubble from Tin Bath Floor in Float Glass Process

在线阅读下载全文

作  者:濮声刚 PU Shenggang(Dongguan CSG Solar Glass Co.,Ltd.,Dongguan 523141,China)

机构地区:[1]东莞南玻太阳能玻璃有限公司,东莞523141

出  处:《玻璃》2024年第12期48-51,共4页Glass

摘  要:锡槽是浮法玻璃生产中的关键热工设备之一,其正常运行对玻璃质量和生产效率具有重要影响。然而,在浮法玻璃生产中,锡槽底部常常出现冒泡现象,导致玻璃板下表面出现严重的开口泡缺陷。通过详细阐述浮法锡槽槽底泡的产生原因,提出相应的预防措施,并探讨了现有的技术创新方法,以减少锡槽槽底泡的产生,提高浮法玻璃生产质量。Tin bath is one of the key thermal equipment in the production of float glass,and its normal run has an important impact on the quality of glass and production efficiency.However,in the production of float glass,bubble often occurs from the the tin bath floor,which results in serious opening bubble defects on the bottom surface of the glass plate.By discussing the causes of the bottom bubble,the corresponding preventive measures are put forward.Some existing technical innovation methods are discussed also in order to avoid the bubble from the bottom of tin bath and improve the quality of float glass.

关 键 词:玻璃 锡槽 槽底泡 

分 类 号:TQ171[化学工程—玻璃工业]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象