反复冷却处理花岗岩的声发射特征及破坏机制研究  

Research on acoustic emission characteristics and failure mechanism of granite treated by repeated cooling

在线阅读下载全文

作  者:朱鹏 王振 武文宾 姚壮壮 王婷 李晓超 陈亮 ZHU Peng;WANG Zhen;WU Wenbin;YAO Zhuangzhuang;WANG Ting;LI Xiaochao;CHEN Liang(Kuche Yushuling Coal Mine Co.Ltd,Kuche 842099,China;Chongqing Research Institute,China Coal Research Institute,Chongqing 400037,China;Chinese Institute of Coal Science,Beijing 100013,China;Department of Mechanical and Electrical Engineering,Ordos Vocational College,Ordos 017010,China)

机构地区:[1]库车市榆树岭煤矿有限责任公司,新疆库车842099 [2]中煤科工集团重庆研究院有限公司,重庆400037 [3]煤炭科学研究总院,北京100013 [4]鄂尔多斯职业学院机电工程系,内蒙古鄂尔多斯017010

出  处:《山东科技大学学报(自然科学版)》2024年第6期1-9,共9页Journal of Shandong University of Science and Technology(Natural Science)

基  金:国家重点研发计划项目(2023YFC3009003);天地科技重点项目(2022-2-TD-ZD008)。

摘  要:为探究反复冷却处理后花岗岩的声发射特征及破坏机制,使用岛津力学试验设备、声发射监测及扫描电子显微镜系统对不同温降等级、冷却循环次数等影响因素处理下的花岗岩试件进行单轴压缩力学试验研究。结果表明:经温降等级10、15和20℃处理后的花岗岩峰值应力分别降低了28.6%、12.9%和6.8%,温降等级越小,峰值应力降低幅值越大。不同冷却处理方式下的花岗岩声发射振铃计数均可划分为平静期和活跃期两个阶段,并随温降等级降低或冷却循环次数增加,花岗岩结构损伤加剧,平静期持续时间延长。花岗岩破坏模式受温降等级和冷却循环次数影响,温降等级10℃时以张拉破坏为主;温降等级15℃时,破坏模式随循环次数增加逐渐由拉剪混合破坏向张拉破坏转变;温降等级20℃时以拉剪混合破坏模式为主。To investigate the acoustic emission characteristics and failure mechanism of granite after repeated cooling treatment,uniaxial compression mechanical tests were conducted on granite specimens treated with different temperature drop levels,cooling cycles,and other influencing factors by using Shimadzu mechanical testing equipment,acoustic emission monitoring,and scanning electron microscopy systems.The experimental results show that the peak stress of granite treated by temperature drop levels of 10,15 and 20℃decreased by 28.6%,12.9%,and 6.8%respectively.The smaller the temperature drop level is,the greater the amplitude of peak stress reduction becomes.The acoustic emission ringing counts of granite under different cooling treatments can be divided into two stages:The calm period and the active period.As the temperature drop level decreases or the cooling frequency increases,the damage to the granite structure intensifies and the duration of the calm period extends.The failure mode of granite is influenced by the temperature drop level and cooling frequency.At a temperature drop of 10℃,tensile failure is the main mode.At a temperature drop of 15℃,the failure mode gradually changes from tensile shear mixed failure to tensile failure with increasing cycles.At a temperature drop of 20℃,tensile shear mixed failure mode is the main mode.

关 键 词:花岗岩 反复冷却 峰值应力 声发射特征 微观结构 破坏机制 

分 类 号:TD325[矿业工程—矿井建设] TU45[建筑科学—岩土工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象