基  金:低碳材料关键应用技术研究及其在汽车上的应用(cstc2021jscx-dxwtBX0022);碳纤维/可回收环氧树脂基复合材料RTM成型汽车件设计、制造基础理论与关键技术(U1909220)。

摘  要:后消费者回收(PCR)材料在汽车保险杠等关键部件上的应用受限于其力学性能不足、油漆附着力差、易起泡等问题,文章研究不同再生料聚丙烯(PP)性能的对比研究,筛选出性能优良的再生料PP,并应用于PP+三元乙丙橡胶(EPDM)-TD20规格材料中,探讨其力学、喷漆及水煮起泡性能。结果表明,再生料的例学性能较新料略低,差示扫描量热仪(DSC)和红外谱图显示,所有试样主要成分均为PP树脂。水煮起泡实验表明,新料PP1>再生料PP2>再生料PP3=再生料PP4;在PP+EPDM-TD20规格体系内,相较于再生料PP3,再生料PP2的力学、耐水煮起泡性能更优,表明再生料PP2表层与油漆之间的表面界面结合力和对油漆中有机小分子的吸附能力较强,在高温水煮条件下不出现小分子脱附,避免因为界面层被剥离出现起泡和起皱等缺陷。当再生料PP2含量为30%,聚烯烃弹性体(POE)含量为20%时,试样的力学性能和喷漆性能最优,百格附着力测试和水煮起泡测试均合格,满足保险杠材料性能要求。The application of post-consumer recycling(PCR)materials in automotive bumpers and other key components is limited by its insufficient mechanical properties,poor paint adhesion,easy foaming and other problems.This paper studies the comparative study of the performance of different recycled polypropylene(PP),and screens out the recycled PP with excellent performance.It is applied to PP+(Ethylene-Propylene-Diene Monomer,EPDM)-TD20,and its mechanics,spray painting and boiling foaming properties are discussed.The results shows that the example properties of the recycled materials are slightly lower than that of the new materials.Differential scanning calorimetry(DSC)and infrared spectroscopy show that the main components of all samples are PP resin.The boiling foaming experiment show that new material PP1>recycled material PP2>recycled material PP3=recycled material PP4.In the PP+EPDM-TD20 system,compared to recycled material PP3,recycled material PP2 exhibits better mechanical properties and resistance to water foaming.This suggests that the surface interface binding force between the recycled material PP2 surface and the paint,as well as its adsorption capacity for small organic molecules in the paint,are stronger.Consequently,small molecule desorption does not occur under high-temperature boiling conditions,thereby avoiding defects such as blistering and wrinkling due to interface layer peeling.When the content of recycled material PP2 is 30%and the content of polyolefin elastomer(POE)is 20%,the mechanical properties and spray painting performance of the sample are optimal,and the sample passes both the 100-cell adhesion test and the boiling foaming test,meeting the performance requirements for bumper materials.

关 键 词:聚丙烯 PCR材料 喷漆保险杠 水煮起泡 

分 类 号:TQ323.4[化学工程—合成树脂塑料工业]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象