Effect of surface roughness on friction and wear behavior of GCr15 bearing steel under different loads  

在线阅读下载全文

作  者:Zhipeng Yuan Zhiguo Jiang Zhenyu Zhou Haidou Wang Jing Li Zhihai Cai Zhiguo Xing Cong Ding Zhongyu Piao 

机构地区:[1]College of Mechanical Engineering,Zhejiang University of Technology,Hangzhou,Hangzhou,Zhejiang 310012,China [2]Key Laboratory of Special Purpose Equipment and Advanced Processing Technology,Ministry of Education and Zhejiang Province,Zhejiang University of Technology,Hangzhou 310012,China [3]National Key Laboratory for Remanufacturing,Army Academy of Armored Forces,Beijing,China [4]National Engineering Research Center for Remanufacturing,Army Academy of Armored Forces,Beijing,China

出  处:《Surface Science and Technology》2024年第1期366-378,共13页表面科学技术(英文)

基  金:financially supported by National Natural Science Foundation of China(NSFC)(52175194,U23A20622,52305222,52205242);Zhejiang Provincial Natural Science Foundation of China(LR23E050002,LQ22E050016);145 Project,NSFC(52130509).

摘  要:To investigate the effects of surface roughness and load on friction and wear behavior,Si3N4 balls and GCr15 bearing steel were selected as the rotating friction pair.The pin-on-disc wear test was carried out under different loads and surface roughness.The experimental results indicate that as the initial surface roughness of the GCr15 bearing steel specimen and applied load increase,the width and depth of the wear tracks also increase,and the wear resistance performance deteriorates.Correlation dimension D and enclosing radius R were used to characterize the running-in quality during the stabilization wear stage.The higher the correlation dimension and the smaller the enclosing radius,the better the running-in quality.The results show that when the initial surface roughness Rq is 0.009μm,and the applied load is 40N,the corresponding correlation dimension is the highest,and the enclosing radius is the smallest,indicating the best running quality.Conversely,when the initial surface roughness is 1.192μm,and the applied load is 20N,the corresponding correlation dimension is the smallest,and the enclosing radius is the largest,indicating the worst running-in quality.The running-in quality is related to the initial surface roughness,with lower initial surface roughness resulting in higher running-in quality.The effect of load on running-in quality is complex due to the complexity of the friction system.

关 键 词:Surface roughness Friction and wear Correlation dimension Enclosing radius Running-in quality 

分 类 号:TG1[金属学及工艺—金属学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象