某超超临界四角切圆锅炉高温腐蚀分析与应对措施  

High-temperature Corrosion Analysis and Countermeasures of a Ultra-supercritical Corner Tangential Boiler

在线阅读下载全文

作  者:秦宁 颜喜 黄军 渠福来 范永胜 饶朗 邓艾东[4] Qin Ning

机构地区:[1]国家能源集团江苏电力有限公司,江苏南京215433 [2]中电华创电力技术研究有限公司,江苏苏州215000 [3]国家能源集团新能源技术研究院有限公司,北京100000 [4]东南大学能源与动力工程学院,江苏南京210000

出  处:《工业控制计算机》2025年第4期114-115,118,共3页Industrial Control Computer

摘  要:某电厂660 MW超超临界直流锅炉在检修期间发现水冷壁高温腐蚀严重,从入炉煤质、运行、炉内动力场等方面分析了高温腐蚀发生的原因,并提出了针对性的治理措施,通过整改后,高温腐蚀情况得到一定缓解。分析方法及治理措施,可为面临相似困扰的发电企业在解决此类问题时提供参考。During the maintenance of a 660 MW ultra-supercritical direct current boiler in a power plant,the high temperature corrosion of the water wall was found to be serious.In this paper,the causes of high temperature corrosion are analyzed from the aspects of coal quality,operation and power field in furnace,and the corresponding treatment measures are put forward.After rectification,the high temperature corrosion has been alleviated to some extent.The analysis method and treatment measures in this paper can provide reference for power generation enterprises facing similar problems in solving such problems.

关 键 词:锅炉燃烧 高温腐蚀 入炉煤质 运行优化 

分 类 号:TK229.2[动力工程及工程热物理—动力机械及工程]

 