提高优结板探伤合格率的技术开发  

Technical Development of Improving Detection Pass Percent of High Quality Structure Plate

在线阅读下载全文

作  者:仉勇[1] 王宏明[1] 

机构地区:[1]鞍钢集团新轧钢股份有限公司

出  处:《鞍钢技术》2003年第4期19-22,共4页Angang Technology

摘  要:通过采取出钢加铝造渣剂、控制浇铸过热度不大于 30℃、根据浇铸断面选择合适的拉速及恒速操作、加大电磁搅拌的电流、定期测量并调整铸机开口度、调整二冷喷嘴状态和提高厚板轧机轧制力等措施 ,显著提高了优结板探伤合格率。The detection pass percent of high quality structure plates is remarkably improved by adopting the measurements such as: adding Al-containing flux while tapping, controlling overheat degree of liquid steel to be ≤30℃ while casting, selecting suitable drawing speed based on casting section and operating at a constant speed, enlarging electric current of electromagnetic mixing, periodically measuring and adjusting tap of continuous caster, adjusting the secondary cooling nozzle status and increasing rolling force of heavy plate mill, etc..

关 键 词:厚板轧制 结构钢 探伤 合格率 技术开发 造渣剂 过热度 拉速 电磁搅拌 

分 类 号:TF762.1[冶金工程—钢铁冶金] TG335.51[金属学及工艺—金属压力加工]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象