自由弧熔融氢方法制备MLC用纳米金属镍粉  被引量:4

Preparation of Nano Nickel Powder for MLCs by Non-confined Arc with Fusible Hydrogen

在线阅读下载全文

作  者:蒋渝[1] 赖庆贵 杨彦明[1] 管登高[1] 陈家钊[1] 涂铭旌[1] 

机构地区:[1]四川大学材料学院金属材料系,四川成都610065 [2]成都宏明电子股份有限公司,四川成都610058

出  处:《电子元件与材料》2003年第12期13-15,共3页Electronic Components And Materials

摘  要:自由弧熔融氢等离子射流方法制备MLC用金属纳米镍粉,平均粒径36.6 nm,粒度呈近似正态分布,94%集中于10~60 nm范围内;分析了制粉空间平均温度及等离子弧柱的轴心线温度,计算过冷温度梯度,指出在弱电离自由弧和强制风冷的情况下仍然可以得到超细纳米金属粉末.Nano nickel powder is prepared by plasma non-confined arc with fusible hydrogen. Its average diameter is 36.6 nanometer. The granularity presents normal distribution and the particles between 10 and 60 nanometer accounts to 94%. The temperature of preparing room and of iron arc were studied, and the overcooling temperature gradient was calculated. Even in the condition of weak arc and strong cooling air, nano powder can be obtained.

关 键 词:金属纳米粉末 制备技术 MLC 金属纳米镍粉 自由弧熔融氢等离子射流方法 

分 类 号:TM241[一般工业技术—材料科学与工程] TB383[电气工程—电工理论与新技术]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象