Microwave dielectric properties of Nextel-440 fiber fabrics with pyrolytic carbon coatings in the temperature range from room temperature to 700℃  被引量:1

Microwave dielectric properties of Nextel-440 fiber fabrics with pyrolytic carbon coatings in the temperature range from room temperature to 700℃

在线阅读下载全文

作  者:宋荟荟 周万城 罗发 卿玉长 陈马林 

机构地区:[1]State Key laboratory of Solidification Processing, Northwestern Polytechnical University

出  处:《Chinese Physics B》2015年第8期594-597,共4页中国物理B(英文版)

基  金:supported by the National Natural Science Foundation of China(Grant No.51072165);the Fund of the State Key Laboratory of Solidification Processing in Northwestern Polytechnical University,China(Grant Nos.KP201307 and SKLSP201313)

摘  要:Pyrolytic carbon(PyC) coatings are deposited on the Nextel-440 fiber fabrics by chemical vapor deposition(CVD).The dielectric properties of the Nextel-440 fiber fabrics with PyC coatings(Nextel-440/PyC) are investigated in a temperature range from room temperature to 700℃ in X-band. Compared with the permittivity of the original Nextel-440 received,the complex permittivity of the Nextel-440/PyC(the real part εand the imaginary part ε), is significantly improved: εof the Nextel-440/PyC has a positive temperature coefficient, in contrast, εof the Nextel-440/PyC exhibits a negative temperature coefficient. Moreover, the reflection loss in units of d B is calculated. The results indicate that the microwave absorbing properties of the Nextel-440/PyC coatings is enhanced at 700℃ compared with that at lower temperatures.Pyrolytic carbon(PyC) coatings are deposited on the Nextel-440 fiber fabrics by chemical vapor deposition(CVD).The dielectric properties of the Nextel-440 fiber fabrics with PyC coatings(Nextel-440/PyC) are investigated in a temperature range from room temperature to 700℃ in X-band. Compared with the permittivity of the original Nextel-440 received,the complex permittivity of the Nextel-440/PyC(the real part εand the imaginary part ε), is significantly improved: εof the Nextel-440/PyC has a positive temperature coefficient, in contrast, εof the Nextel-440/PyC exhibits a negative temperature coefficient. Moreover, the reflection loss in units of d B is calculated. The results indicate that the microwave absorbing properties of the Nextel-440/PyC coatings is enhanced at 700℃ compared with that at lower temperatures.

关 键 词:pyrolytic carbon coating chemical vapor deposition dielectric property 

分 类 号:TS195.5[轻工技术与工程—纺织化学与染整工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象