Experimental Study of the Influence of Intrinsic Parameters on the Thermal Reactivity of Sawdust, Polyethylene Terephthalate and Composite  

Experimental Study of the Influence of Intrinsic Parameters on the Thermal Reactivity of Sawdust, Polyethylene Terephthalate and Composite

在线阅读下载全文

作  者:Ange Brel Boukongou Timoléon Andzi Barhé Ange Brel Boukongou;Timoléon Andzi Barhé(Applied Chemistry Research Laboratory (LARCA), Ecole Normale Supérieure (ENS), Marien NGOUABI University (UMNG), Brazzaville, Congo)

机构地区:[1]Applied Chemistry Research Laboratory (LARCA), Ecole Normale Supérieure (ENS), Marien NGOUABI University (UMNG), Brazzaville, Congo

出  处:《Journal of Materials Science and Chemical Engineering》2024年第3期9-20,共12页材料科学与化学工程(英文)

摘  要:Several works have been based on the study of thermal variations in biomass to derive more valuable products such as fuels capable of replacing oil in the event of a crisis or activated carbon used as an adsorbent material, widely used in industry for the elimination of unwanted materials, both in liquid and gaseous environments. A study of thermal parameters such as: heating speed, retention time, drying temperature, carbonization temperature, particle size, was carried out with the aim of determining the characteristic factors of the carbonization of Polyethylene terephthalate (PET), sawdust (SC) and sawdust/polyethylene terephthalate (CPS) mixture. The results of the immediate analysis revealed a very low level of ash in PET (0.013%) compared to the level of ash in sawdust (2.9%), as well as a high level of fixed carbon (82.960%), which suggests the presence of mineral oxides and a significant carbon matrix unlike PET, which indicates a very significant organic matrix (essentially made up of organic matter) with the absence of mineral oxides. The study of thermal parameters showed the water loss from Sawdust (SC) and the Sawdust/Polyethylene terephthalate (CPS) mixture, an increase with temperature, unlike that of PET whose variation is essentially zero. Without heat treatment, sawdust alone contains approximately 7% water. The optimal drying temperature for this study is 110˚C for a stay of 24 hours. It appears that the largest mass losses for the PET samples are between 87.19% and 96.05%, followed by that of the mixture, between 47.33% and 64.37%. And the lowest are observed, those of sawdust (from 24.02% to 62.6%). However, here we can say that the influence of the mass is not great, given the slight difference between the losses by temperature. The results of the study of the influence of grain size showed that the differences are insignificant, even if we vary the diameter of the grains from simple to triple. To better minimize physical constraints such as the intragranular diffusibility of the volatile Several works have been based on the study of thermal variations in biomass to derive more valuable products such as fuels capable of replacing oil in the event of a crisis or activated carbon used as an adsorbent material, widely used in industry for the elimination of unwanted materials, both in liquid and gaseous environments. A study of thermal parameters such as: heating speed, retention time, drying temperature, carbonization temperature, particle size, was carried out with the aim of determining the characteristic factors of the carbonization of Polyethylene terephthalate (PET), sawdust (SC) and sawdust/polyethylene terephthalate (CPS) mixture. The results of the immediate analysis revealed a very low level of ash in PET (0.013%) compared to the level of ash in sawdust (2.9%), as well as a high level of fixed carbon (82.960%), which suggests the presence of mineral oxides and a significant carbon matrix unlike PET, which indicates a very significant organic matrix (essentially made up of organic matter) with the absence of mineral oxides. The study of thermal parameters showed the water loss from Sawdust (SC) and the Sawdust/Polyethylene terephthalate (CPS) mixture, an increase with temperature, unlike that of PET whose variation is essentially zero. Without heat treatment, sawdust alone contains approximately 7% water. The optimal drying temperature for this study is 110˚C for a stay of 24 hours. It appears that the largest mass losses for the PET samples are between 87.19% and 96.05%, followed by that of the mixture, between 47.33% and 64.37%. And the lowest are observed, those of sawdust (from 24.02% to 62.6%). However, here we can say that the influence of the mass is not great, given the slight difference between the losses by temperature. The results of the study of the influence of grain size showed that the differences are insignificant, even if we vary the diameter of the grains from simple to triple. To better minimize physical constraints such as the intragranular diffusibility of the volatile

关 键 词:Intrinsic Parameters Thermal Reactivity SAWDUST Polyethylene Terephthalate COMPOSITE 

分 类 号:TQ5[化学工程]

 