Elaboration and Characterization of a Fiber Composite Material Made of Petioles of the <i>Elaeis guineensis</i>(Oil Palm)  

Elaboration and Characterization of a Fiber Composite Material Made of Petioles of the <i>Elaeis guineensis</i>(Oil Palm)

在线阅读下载全文

作  者:Ze Eric Parfait Tchotang Théodore Souck Joseph Loic Nfor Clins Wiryikfu Pondi Joseph Mpoung Léon Arnaud Ze Eric Parfait;Tchotang Théodore;Souck Joseph Loic;Nfor Clins Wiryikfu;Pondi Joseph;Mpoung Léon Arnaud(Local Materials Promotion Authority, Yaoundé, Cameroon;National Advanced School of Engineering Yaoundé, University of Yaoundé 1, Department of Mechanical Engineering, Laboratory of Civil Engineering and Mechanics, Yaoundé, Cameroon)

机构地区:[1]Local Materials Promotion Authority, Yaoundé, Cameroon [2]National Advanced School of Engineering Yaoundé, University of Yaoundé 1, Department of Mechanical Engineering, Laboratory of Civil Engineering and Mechanics, Yaoundé, Cameroon

出  处:《Open Journal of Composite Materials》2020年第4期106-117,共12页复合材料期刊(英文)

摘  要:The aim of this study is to characterize physically and mechanically a polyester/fiber palm petiole composite material. This work made it possible to provide the local database of composite materials but also to develop agricultural waste. According to BSI 2782 standard three formulations [A (10% fiber, 90% polyester);B (20% fiber, 80% polyester) and C (30% fiber, 70% po</span><span style="font-family:Verdana;">lyester)]. Water Absorption rate, density, compressive and three points</span><span style="font-family:Verdana;"> bending tests are carried out on the samples obtained by the contact molding method for each formulation. The material composite obtained by adding fibers from palm oil petiole has a density of 17.98% lower than the one made of pure polyester. Fiber reinforcement rate has no impact on the density of the composite. Formulation A most absorbs water while formulation C has good tensile/compression characteristics and the greatest breaking stress in bending among the three formulations.The aim of this study is to characterize physically and mechanically a polyester/fiber palm petiole composite material. This work made it possible to provide the local database of composite materials but also to develop agricultural waste. According to BSI 2782 standard three formulations [A (10% fiber, 90% polyester);B (20% fiber, 80% polyester) and C (30% fiber, 70% po</span><span style="font-family:Verdana;">lyester)]. Water Absorption rate, density, compressive and three points</span><span style="font-family:Verdana;"> bending tests are carried out on the samples obtained by the contact molding method for each formulation. The material composite obtained by adding fibers from palm oil petiole has a density of 17.98% lower than the one made of pure polyester. Fiber reinforcement rate has no impact on the density of the composite. Formulation A most absorbs water while formulation C has good tensile/compression characteristics and the greatest breaking stress in bending among the three formulations.

关 键 词:ELABORATION CHARACTERIZATION Physico-Mechanical Composite POLYESTER PETIOLES Oil Palm 

分 类 号:TB3[一般工业技术—材料科学与工程]

 