相关期刊:《Journal of Wuhan University of Technology(Materials Science)》《Science Bulletin》《Journal of Iron and Steel Research International》《Progress in Natural Science:Materials International》更多>>
Funded by the Natural Science Foundation of Shanxi Province(No.202203021211093)。
The experiment employed the use of melt purification and cyclic superheating technique to achieve maximum undercooling of Ni65Cu31Co4 alloy at 300K.Simultaneously,high-speed photography techniques were used to capture...
Funded by the Basic Research Project in Shanxi Province(No.202103021224183)。
Through the use of purification and recirculation superheating techniques on molten glass,the Ni65Cu33Co2 alloy was successfully undercooled to a maximum temperature of 292 K.High-speed photography was employed to cap...
Project(50874073) supported by the National Natural Science Foundation of China;Project(2011CB610405) supported by the National Basic Research Program of China;Project(2011M500074) supported by China Postdoctoral Science Foundation
A series of Co-Sn alloys with Sn content ranging from 12% to 32%(mole fraction) were undercooled to different degrees below the equilibrium liquidus temperature and the solidification behaviors were investigated by ...
Item Sponsored by European project "MAGPRO"(RFSR-CT-2006-00019);National Basic Research Program of China(Grant No.2011CB610404)
The recalescence behavior of undercooled Co-Sn alloys under static magnetic fields was investigated using glass slag fluxing technique in a 12T superconducting magnet.Results indicated that the nucleation temperature ...
Project supported by the National Natural Science Foundation of China (Grant No. 59701003) and Aeronautics Fundamental Science Foundation of China (Grant No. 98G53089).
By cyclic superheating incorporated with glass fluxing denucleation method the Fe82B17Si1 eutectic alloy was undercooled up to △T = 342 K. The relations between recalescence behavior and solidification structures wer...
The solidification characteristics of highly undercooled Cu-7.77% Co peritectic alloy has been examined by glass fluxing technique. The obtained undercoolings vary from 93 to 203 K(0.14 T_L). It is found that the a(Co...
Financilly suported by the National Natural Science Foundation of China
Fluxing of 5 g bulk melt Ni77Si13B10 permits high undercoolings to be attained prior to nu-cleation onset.Investigations of grain refinement in the bulk undercooled alloy as a function ofundercooling,recalescence beha...
One,two and three recalescence events in the solidification of highly undercooled Ni_68B_21Si_11 alloy melt and the conditions of undercooling together with the effect on solidification morphologies were revealed.The ...