Transient liquid phase(TLP)bonding was investigated in Hastelloy-X samples with different filler metal thicknesses(20,35,50,65,and 100μm)and holding time(5,20,80,320,and 640 min)to obtain optimum bonding parameters.M...
Underwater friction stir processing was performed on commercially pure copper with a purity of 99.8% and a copper-zinc alloy(brass). The tool was made of tungsten carbide in the threaded cone form. Friction stir proce...
The 2024Al/Gr/SiC hybrid composite plates with 5%-10% SiC particles (volume fraction) and 3%-6% flaky graphite (Gr) (volume fraction) were fabricated by vacuum hot pressing and hot extrusion processing. The effe...