作 者:张宏昌[1] 赵卫国[2] 杜建斌[1] 张帅[1] 潘海波[1] 相聪[1] 王振忠[1] 吴尚超[1]
机构地区:[1]河北钢铁集团有限公司邯钢公司中板厂,河北邯郸056003 [2]河北钢铁集团有限公司邯钢公司
出 处:《冶金自动化》2010年第1期22-25,68,共5页Metallurgical Industry Automation
摘 要:宽厚板轧制时,钢板头部咬入冲击将对轧机弹跳产生影响,若不采取补偿措施,头部厚度将超差严重。邯郸钢铁集团有限责任公司3 500 mm轧机原来虽采用了三角形头部厚度补偿模型,但头部厚度超差仍达0.5 mm左右。通过对钢板头部厚度数据的分析,找出了头部厚度波动规律,提出了变斜率头部厚度补偿改进模型。采用该模型并严格执行咬入速度制度后,头部厚度超差减小到0.2 mm左右。The impact of head biting influences spring of wide and heavy plate rolling mill.Without taking a measure,oversize in head thickness of plate is very serious.Although a triangular head thickness compensation model was adopted in 3 500 mm rolling mill of Handan Iron and Steel Group Co.,Ltd.,oversize of head thickness was still up to around 0.5 mm.Through analysis of plate head thickness data,common trend of head thickness fluctuation is found and a slope-variable compensation model for head thickness control...
分 类 号:TG334.9[金属学及工艺—金属压力加工]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.229