八钢0~#连铸机工艺优化及效果  

Process Optimization of 0~# Continuous Caster in Bayi Steel and Its Effect

在线阅读下载全文

作  者:王建新[1] 徐逸飞[1] 

机构地区:[1]宝钢集团新疆八一钢铁有限公司炼钢厂,新疆乌鲁木齐830022

出  处:《宝钢技术》2010年第6期57-60,共4页Baosteel Technology

摘  要:介绍八钢一炼钢0#连铸机为提高产量而采取的一系列改进措施:通过扩大中间包上水口直径,优化二冷配水制度,合理分配各冷却段水的比例等,取得了较好的效果。0#连铸机平均拉速由2008年的3.04 m/min提高到2009年的3.21 m/min;产量大大提高,年产量由2008年的1005 179.926 t,提高到2009年的1040 853.075 t,提高了35 673.149 t,生产、铸坯质量比较稳定。A series of improvement measures for increasing output of the 0# continuous caster in Bayi Iron & Steel Co.,Ltd.,(Bayi Steel for short) were introduced.These measures include enlarging diameter of the tundish upper nozzle,optimizing the water distribution of the secondary cooling scheme,allocating the water proportion reasonably for each cooling section,etc.A better result was gained.The average casting speed was increased from 3.04 m/min in 2008 to 3.21 m/min in 2009.Production of the caster grew from 1 00...

关 键 词:拉速 作业率 二冷制度 中间包 上水口 

分 类 号:TF777[冶金工程—钢铁冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象