Cr12MoV钢CD渗碳后等温淬火组织中的残余奥氏体  

The Retained Austenite Emerged in the Austempered Structure after CD Carburizing

在线阅读下载全文

作  者:朱穗东[1] 刘春梅[1] 丛欣[1] 宁玫 李宜增 

机构地区:[1]天津理工学院一分院,天津无缝钢管公司

出  处:《材料工程》1995年第4期27-29,共3页Journal of Materials Engineering

摘  要:Cr12MoV钢经渗碳等温淬火,渗层和心部组织中的残余奥氏体已占较大比例,但这两区域的γ'数量变化规律相反,反映了该区域成分和组织变化的特殊性,从而构成高碳高合金钢CD渗碳等温淬火组织的一个重要研究方面。s a high carbon content and high alloy element alloy steel, Cr 12 MoV steel has been carburized fol-lowed by austemporing.There is a relatively large quantity of retained A both in the inside structure and surface layer, but the quantity of retained A in these two positions change.in reverse pattern.This is caused by speciality of phase and composition in these two parts. The study on retained A is a important aspect in the structure of CD carburizing followed by austempering in high carbon and high alloy element alloy steel.

关 键 词:CD渗碳 等温淬火 残余奥氏体 CR12MOV钢 

分 类 号:TG142.14[一般工业技术—材料科学与工程] TG161.81[金属学及工艺—金属材料]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象