THPC鞣制作用的研究  被引量:5

Study on Tanning Action of THPC

在线阅读下载全文

作  者:史楷岐[1] 蒋岚[1] 李亚[1] 单志华[2] 邵双喜[1] 

机构地区:[1]宁波工程学院应用化学研究所,浙江宁波315016 [2]四川大学皮革化学与工程教育部重点实验室,四川成都610065

出  处:《中国皮革》2006年第9期9-10,15,共3页China Leather

基  金:国家"十五"863计划(2003AA647020);浙江省自然科学基金(X403005);宁波市科技计划资助项目

摘  要:考察了不同pH条件下,THPC对皮粉的鞣制作用。应用碘滴定法和磷钼蓝法测定THPC在鞣后皮粉中的含量。结果表明:当鞣制体系pH为10.0时,皮粉对THPC的吸附结合量较大,达到皮粉质量的50.13%;此时鞣制后皮粉的变性温度(TD)相对较高,为77.8℃。因此,THPC作为单一的主鞣剂,难于满足无铬皮革的鞣制要求。The tanning actions of THPC under different pH values were studied, lodometric titration and phosphor molybdenum blue spectrophotometry were used to determine the THPC quantity bounded by hide powder. It shows that when pH value is 10.0, the maximum combination ratio (50.13 % ) of THPC; combined with hide power is obtained. Also the protein denaturation temperature (77.8℃)is the highest. Therefore THPC cannot be used as single tanning agent in tanning proceeds, for it cannot satisfy the normal standards of chrome- free leathers.

关 键 词:THPC 鞣制 PH 变性温度(TD) 皮粉 

分 类 号:TS543[轻工技术与工程—皮革化学与工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象