摘  要:研究20钢,45钢经奥氏体离子氮碳共渗后的耐磨性和抗咬合性,并与普通离子氮碳共渗后的作了比较,试验表明:在570—700℃范围内进行奥氏体离子氮碳共渗后,其耐磨性和抗咬合性以630℃处理时为最佳,660℃最差,而570—600℃介于二者之间,通过适当提高共渗温度在提高渗速从而缩短共渗时间的同时,可以提高耐磨损性能。Studies of the wear resistance and anti-adhesion of 20# and 45# steel formed in austenitic ion-nitrocarburising and comparisons to the general ion-nitrocarburising are presented in this thesis. The experiment shows that austenitic ion-nitrocarburising can be carried out at 570-700℃, its wear resistance and anti-adhesion is the best at 630℃, the worst at 660℃ and the mediate at 570-600℃. The wear behaviour can be improved by raising processing temperature properly and speeding up the process, future shortening processing time.

关 键 词:奥氏体 氮碳共渗 耐磨性 抗咬合性  

分 类 号:TG161.82[金属学及工艺—热处理]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象