单板旋切厚度均匀性分析及改进措施  被引量:12

Analysis of the Evenness of Venner Peeling Thickness and Improving Measures

在线阅读下载全文

作  者:张少纯[1] 朱孝生[1] 巴兴强[1] 张绍群[1] 鹿占山 闫玉祥 

机构地区:[1]东北林业大学 [2]内蒙古伊图里河林业局 [3]内蒙古乌尔旗汗林业局

出  处:《东北林业大学学报》1997年第2期75-77,共3页Journal of Northeast Forestry University

摘  要:通过对木段旋切时的受力状况进行分析及计算,指出单板厚度不均,即中间薄,两边厚,是旋切时木段产生弯曲挠度所致。通过实验也证实了这个结论。并指出旋切时采用防弯压辊是提高单板旋切精度,进而提高胶合板厚高均匀性的关键。建议采用带有防弯装置的旋切机生产单板。Through analysis and calculation of suffer force condition in peeling log, this article pointed out the peeling thickness uneven, that is the outer sides are thick but the middle is thin, is result of the bending deflection in peeling log. The result has been confirmed by experiment. Adopting the anti-bend press roll is the key to improve the precision of veneer peeling and the thickess eveneess of the plywood. Rotary cut machine with anti-bend press roll should be adopted in veneer producing for saving wood resources.

关 键 词:木板 单板旋切 受力 防弯压辊 

分 类 号:TS653.2[轻工技术与工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象