软质纤维板的闭式喷蒸热压工艺  

Enclosing a Steam Injection Press for Manufacturing Low Density Fiberboard

在线阅读下载全文

作  者:李霞镇[1] 任海青[1] 谢力生[2] 徐明[1] 

机构地区:[1]中国林科院木材工业研究所;国家林业局木材科学与技术重点实验室,北京100091 [2]中南林业科技大学材料科学与工程学院,湖南长沙410006

出  处:《木材工业》2008年第3期41-43,共3页China Wood Industry

基  金:公益性行业科研专项基金(200704013)

摘  要:闭式喷蒸热压克服了蒸汽泄漏的缺点,适合用于软质纤维板的生产。本试验参照有关资料,确定了热压工艺参数为:热压温度160℃、施胶量10%、喷蒸时间10 s、热压时间10 s/mm进行试验,按此参数压制的软质纤维板,板材性能符合GB/T 17657-1999要求。This study focused on enclosing a steam-injection press, to eliminate any steam leakage, to produce low density (0. 3 g/cm^3) fiberboard. After reviewing this technology from previous studies, the authors designed an orthogonal experiment to optimize the process parameters for making low density fiberboard. The results indicated that when 10% resin content, 160 ℃ pressing temperature, 10 s steam injection time, and 10 s/mm pressing time were used, the properties of fiberboards met the reouirements of national standard GB/T 17567-1999.

关 键 词:闭式 喷蒸热压 软质纤维板 热压工艺 

分 类 号:TS653.6[轻工技术与工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象