结合鞣机理研究──稀土-植鞣革特征  被引量:1

Studies on The Mechanism of Combination Tanning -Characteristics of Leather Tanned With Rare Earth -Vegetable Tannin Extract

在线阅读下载全文

作  者:单志华[1] 何先祺[1] 

机构地区:[1]四川联合大学皮革化学与工程国家专业实验室,成都610065

出  处:《皮革科学与工程》1998年第1期1-4,共4页Leather Science and Engineering

摘  要:本文涉及了稀土-植物鞣剂的化学研究.鞣法研究及革的物理机械性能。单独稀土鞣革的收缩温度为62℃.植鞣的收缩温度为83℃,而两者结合鞣为102℃,并且这种结合鞣革有良好的手感及强度。研究表明这种结合鞣在制革工业中有重要的现实意义。This paper involves the studies of chemisty and technology on combination tanning of rare earth - vegetable tanning extract and physical - mechanical properties of the combination tanning leather. The leather tanned with rare earth has a shrinkage temp, 62℃ and 83℃ with vegetable tanning extract and then 102℃ with rare earth - vegetable tannin extract.The combination tanning leather has also good handle and strength. The results show that this kind of combination tanningmethod has practical value in leather industry.

关 键 词:稀土 植物鞣剂 结合鞣 机理 鞣制化学 

分 类 号:TS513[轻工技术与工程—皮革化学与工程] TQ941[化学工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象