机构地区:[1]同济大学污染控制与资源化研究国家重点实验室,上海200092
出 处:《环境科学》2009年第8期2366-2370,共5页Environmental Science
基 金:霍英东基金项目(101080)
摘 要:聚羟基烷酸酯(polyhydroxyalkanoate,PHA)是一种生物可降解塑料,利用活性污泥合成PHA具有操作方便的优点.本研究对长期驯化的厌氧-好氧活性污泥工艺在厌氧条件下及好氧活性污泥工艺在好氧条件下利用乙酸合成PHA进行了比较分析,发现好氧活性污泥可以合成较多的PHA.在此基础上,研究了好氧条件下乙酸加入次数、乙酸浓度及硝化抑制剂(丙烯基硫脲,ATU)对PHA合成的影响,结果表明,将乙酸分3次加入到反应器、乙酸浓度为2 925 mg/L及加入6.74 mg/L ATU时,可以使污泥挥发性悬浮固体物中PHA的含量达到56.3%.Polyhydroxyalkanoate (PHA) is a type of biodegradable plastics. The synthesis of PHA by activated sludge has the advantage of easy operation. With acetic acid as the carbon source, the anaerobic synthesis of PHA in the anaerobic-aerobic activated sludge system was compared with the aerobic one in the aerobic sludge system. It was observed that the aerobic PHA synthesis was greater than the anaerobic one. The influences of acetic acid addition frequency, acetic acid concentration and allyl thiourea (ATU) on aerobic PHA synthesis were further investigated. The results showed that the PHA content accounting for volatile suspended solids reached 56.3 % under conditions of acetic acid addition with frequency of 3, acetic acid concentration of 2 925 mg/L, and ATU concentration of 6.74 mg/L.
关 键 词:活性污泥 聚羟基烷酸酯 好氧合成 乙酸 丙烯基硫脲
分 类 号:X172[环境科学与工程—环境科学]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.249