超声波协同催化氧化法脱除废旧轮胎热裂解油中的硫  

Desulfurization of Pyrolysis Oil from Waste Tires by Catalytical Oxidation Process Cooperated with Ultrasonic Wave

在线阅读下载全文

作  者:郑育英[1] 王俏运[1] 黄慧民[1] 杨红梅[1] 

机构地区:[1]广东工业大学轻工化工学院,广东广州510006

出  处:《化工环保》2009年第6期541-544,共4页Environmental Protection of Chemical Industry

摘  要:采用超声波氧化与催化氧化脱硫技术相结合,脱除废旧轮胎热裂解油中的硫,对脱硫工艺进行了研究。最佳操作条件为:超声波声强0.25 W/cm^2,超声时间10 min,V(H_2O_2):V(油)=0.04,V(CH_3COOH):V(H_2O_2)=0.5,V(FeSO_4·7H_2O):V(H_2O_2)=0.15。在上述最佳操作条件下,进行4次脱硫,可使热裂解油中硫质量分数降至0.21%,脱硫率达到72%。Pyrolysis oil from waste tires was desulfurated by ultrasonic oxidation - catalytic oxidation process. The optimum operation conditions are as follows: The intensity of ultrasonic wave is 0.25 W/cm^2, the ultrasonic reaction time is 10 min, V( H2O2 ) : V(oil) = 0.04, V(CH3COOH) : V(H2O2) = 0.5, V(FeSO4 . 7H20) : V( H2O2 ) = 0. 15. After the pyrolysis oil was desulfurated for 4 times under the optimum operation conditions, the mass fraction of sulfur in the pyrolysis oil is decreased to 0.21% and the desulfurization rate is 72%.

关 键 词:超声波 催化氧化 脱硫 热裂解油 

分 类 号:X382.1[环境科学与工程—环境工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象