The organic diamond disk(ODD)for dressing polishing pads of chemical mechanical planarization  被引量:1

The organic diamond disk(ODD)for dressing polishing pads of chemical mechanical planarization

在线阅读下载全文

作  者:Chou Cheng-Shiang Sung James C. Pai Yang-Liang Sung Michael 

机构地区:[1]KINIK Company,64,Chung-San Rd.,Ying-Kuo [2]National Taiwan University [3]National Taipei University of Technology [4]Advanced Diamond Solutions,Inc.,351 King Street Suite 813,San Francisco,CA 94158,U.S.A.

出  处:《金刚石与磨料磨具工程》2008年第S1期126-129,共4页Diamond & Abrasives Engineering

摘  要:Diamond pad conditioners can determine the efficiency of CMP processes and the quality of polished wafers.The polishing rate of a wafer is dependent on the amplitude(height) of pad asperities.The polishing uniformity is controlled by the frequency(density) of such asperities.Current diamond pad conditioners cannot dress the pad to produce microns sized asperities at high density.This is because the tips of diamond grits cannot be leveled to the same height so the grooved pad top is uneven with excessive asperities that may ruin the wafer and under sized asperities that is easily glazed. New designs of diamond pad conditioners have markedly improved the leveling of diamond tips.Organic diamond disks(ODD) are manufactured by reverse casting of polymers.Due to the uniform spacing of diamond grits and their controlled tip heights,none of the diamond grits will be overly stressed.Moreover,all diamond grits are sharing the dressing work.Consequently,the number of working grits of ODD is significantly higher than conventional designs.Moreover,because no diamond will cut pad unecessarily,the pad life is greatly lengthened.Furthermore,due to the uniform distribution of pad asperities,the slurry will be held efficiently so the run off is avoided.As a result,the slurry usage is reduced.ODD is therefore a significant savor of CMP consumables for semiconductor manufacture.Diamond pad conditioners can determine the efficiency of CMP processes and the quality of polished wafers.The polishing rate of a wafer is dependent on the amplitude(height) of pad asperities.The polishing uniformity is controlled by the frequency(density) of such asperities.Current diamond pad conditioners cannot dress the pad to produce microns sized asperities at high density.This is because the tips of diamond grits cannot be leveled to the same height so the grooved pad top is uneven with excessive asperities that may ruin the wafer and under sized asperities that is easily glazed. New designs of diamond pad conditioners have markedly improved the leveling of diamond tips.Organic diamond disks(ODD) are manufactured by reverse casting of polymers.Due to the uniform spacing of diamond grits and their controlled tip heights,none of the diamond grits will be overly stressed.Moreover,all diamond grits are sharing the dressing work.Consequently,the number of working grits of ODD is significantly higher than conventional designs.Moreover,because no diamond will cut pad unecessarily,the pad life is greatly lengthened.Furthermore,due to the uniform distribution of pad asperities,the slurry will be held efficiently so the run off is avoided.As a result,the slurry usage is reduced.ODD is therefore a significant savor of CMP consumables for semiconductor manufacture.

关 键 词:CMP DIAMOND DRESSER pad CONDITIONER epoxy 

分 类 号:TG73[金属学及工艺—刀具与模具]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象