电站面式减温器辐射状裂纹成因分析及预防对策  被引量:1

Radial cracks analysis and preventive measures for the plant surface desuperheater

在线阅读下载全文

作  者:崔靖渝[1] 王猛[1] 杨建飞[1] 蒋玲娣[1] 郑玉卿[1] 

机构地区:[1]湖州师范学院信息与工程学院,浙江湖州313000

出  处:《现代机械》2014年第2期60-62,共3页Modern Machinery

基  金:2013年浙江省大学生科技创新活动计划项目-新苗人才计划(2013R425026)

摘  要:针对同一台电站面式减温器连续两年在蒸汽引出管孔处出现辐射状裂纹,本文从面式减温器高温高压下的材料特性、理论应力计算和工作环境三个方面作了详细的分析和讨论,获得了蒸汽引出管孔处所承受的应力值,同时校核了电站面式减温器在实际运行过程中的结构强度,从而分析了面式减温器产生辐射状裂纹的主次因素,最后提出了相应的预防对策和改进建议。For the radial cracks occurred on the steam outlet hole surroundings in the same surface desuperheater located in a power plant 'after its updating two years ago, this article discussed the crack development mechanism from three aspects of material properties under high temperature and pressure, theoretical calculations and work environment, getting the stress values of the steam extraction hole and checking the structural strength of the surface desuperheater in actual working. And it distinguished the primary and secondary factors to cause the radial cracks. Finally, it proposed the corresponding preven- tion measures and improvement suggestions.

关 键 词:面式减温器 辐射状裂纹 强度校核 预防对策 

分 类 号:TS642[轻工技术与工程] TH114[机械工程—机械设计及理论]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象