超高性能混凝土轴拉性能试验  被引量:224

Axial Tensile Behavior Test of Ultra High Performance Concrete

在线阅读下载全文

作  者:张哲[1] 邵旭东[1,2] 李文光[1] 朱平[1,2] 陈洪[1,2] 

机构地区:[1]湖南大学土木工程学院,湖南长沙410082 [2]湖南大学风工程与桥梁工程湖南省重点实验室,湖南长沙410082

出  处:《中国公路学报》2015年第8期50-58,共9页China Journal of Highway and Transport

基  金:国家自然科学基金项目(51178177;51378194);交通运输部重大科技专项项目(2011318494160)

摘  要:为提高超高性能混凝土(UHPC)的初裂应变,在基体中混合掺入平直钢纤维和端钩钢纤维,考虑纤维掺量和形状的影响,对掺混合纤维的UHPC进行了轴拉试验。采用控制变量法,将4种含不同纤维掺量的UHPC材料的轴拉特征参数进行了对比分析。基于实测曲线,提出了包含应力-应变关系和应力-裂缝宽度关系的两阶段拉伸本构模型。研究结果表明:不同纤维掺量的UHPC材料的拉应力-伸长曲线随多元开裂均呈明显的应变硬化特性;当钢纤维掺量由2%增至3.5%时,可视初裂应变增加201%,且端钩纤维的增强效率为平直纤维的3.52倍;含3.5%纤维掺量的UHPC材料的可视初裂应变和极限应变分别高达1.777×10-3和1.941×10-3,均与普通钢筋屈服应变(2×10-3)接近,可视初裂前UHPC材料能与钢筋协同变形;UHPC受拉本构关系模型与试验数据均符合较好。To enhance the crack-observed strain of Ultra High Performance Concrete (UHPC), hybrid steel fibers including straight fibers and hooked-end fibers were blended into the matrix of UHPCs. Considering the influence of fiber content and fiber shape, axial tensile test of UHPC with hybrid fibers was investigated. With control variable method, axial tensile characteristic parameters of UHPCs with four different fiber contents were compared. Based on measured tensile stress-elongation curves, a two-stage tensile constitutive model of UHPC comprised of a stress-strain response and a stress-crack opening relationship was proposed. The results show that tensile stress-elongation curves of UHPC with different hybrid fiber contents apparently exhibit strain-hardening behavior with multiple cracking. As the fiber content increases from 2 to 3. 5%, the crack-observed strain considerably improves by 201% and the enhancement of hooked-end fibers is 3.52 times greater than that of the straight fibers. With addition of 3.5 hybrid fibers by volume, the strains, corresponding to the observed cracking and stress softening, are 1. 777× 10-3^ and 1. 941 X 10-3^ respectively, which approach the yielding strain of common reinforcing bar (2 × 10-3^). coordinately deform with reinforcing stee proposed UHPC tensile constitutive mod Before an occurrence of a visible crack, UHPC can 1. Finally, test data are satisfactorily approximate to the

关 键 词:桥梁工程 超高性能混凝土 直接拉伸试验 拉伸性能 应变硬化 

分 类 号:U444[建筑科学—桥梁与隧道工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象