65mm红柳桉锯材干燥工艺试验研究  

Study on Drying Technology of 65mm Thick Shorea spp.Lumber

在线阅读下载全文

作  者:孟杨[1] 赵庚[1] 褚俊[1] 陈广元[1] 

机构地区:[1]东北林业大学

出  处:《林产工业》2015年第10期27-30,共4页China Forest Products Industry

基  金:林业公益性行业科研专项经费项目(201304502)

摘  要:以65mm红柳桉锯材为研究对象,采用4种不同的干燥基准对其进行初步探究。结果表明:干燥前期表层含水率下降速度快,芯层含水率向表层迁移的速度慢,前期温度过高,干燥速度过快,木材容易开裂。采用波动干燥基准,利用温度监控设备控制干燥过程的实施,可以有效地减少65mm红柳桉干燥过程中的开裂现象,缩短干燥周期。65mm thick Shorea spp. lumber and four different kinds of drying schedules were used to explore the lumber drying process. The results indicated that surface moisture content of the lumber decreased faster but moisture migration from core layer to surface layer was slower.The experiments showed that the lumber cracked easily when initial temperature was too high and drying rate was too fast. The fluctuant drying process with temperature monitoring device controlling the implementation of the drying process can effectively reduce 65mm thick timber cracking in Shorea spp. drying process and shorten the drying period.

关 键 词:红柳桉 锯材 干燥基准 波动基准 

分 类 号:S784[农业科学—林学] TS653.2[轻工技术与工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象