大方坯铸坯表面夹渣的实践原因分析  

Analysis on the Practice of Slag Inclusion on the Surface of Bloom

在线阅读下载全文

作  者:郝志伟[1] 赵永龙 韩小强[1] HAO Zhi-wei ZHAO Yong-long HAN Xiao-qiang(Hebei Jinxi Iron and Steel Group Limited by Share Ltd., Tangshan 064300, Chin)

机构地区:[1]河北津西钢铁集团股份有限公司,河北唐山064300

出  处:《甘肃冶金》2017年第6期20-22,共3页Gansu Metallurgy

摘  要:大方坯表面夹渣分为两种类型,一类是铸坯角部卷渣、二类是铸坯的大面镶嵌渣铁块。而结晶器液面波动过大和保护渣的性能不良对这两种夹渣类型都有很大的影响。根据夹渣的不同类型和造成夹渣的不同形式,主要从工艺上和保护渣性能上采取相应的措施解决大方坯表面夹渣问题,提高铸坯的收得率。The bloom surface slag is divided into two types, one is the slab corner rolling slag and two is the large mosaic slag casting iron. However, the fluctuation of mold surface and the poor performance of the slag have great influence on the two types of slag. According to the different types of slag and the different forms of slag inclusion, the corresponding meas- ures were taken to solve the problem of slag inclusion on the surface of the billet, and the yield of the slab was improved.

关 键 词:表面夹渣 液面波动 保护渣 收得率 

分 类 号:TF777.2[冶金工程—钢铁冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象