邯宝1号高炉炉温大凉后应对措施  被引量:1

Countermeasures for Hanbao No.1 Blast Furnace after Cooling

在线阅读下载全文

作  者:刘志福 王拓 Liu Zhifu;Wang Tuo(Hanbao Ironmaking Plant,HBIS Group Handan Iron and Steel Company,Handan Heibei 056015)

机构地区:[1]邯钢公司邯宝炼铁厂,河北邯郸056015

出  处:《山西冶金》2020年第4期170-171,共2页Shanxi Metallurgy

摘  要:邯钢西区1号高炉因长期配吃湿焦炉缸不活跃,炉前倒场后出铁不顺,炉内频繁出气流,造成炉温过低,主沟渣沟冻结。本文对造成炉温大凉的原因及应对措施进行了总结,通过优化出铁方案,合理控制各项操作参数,快速恢复到正常生产水平,取得良好效果。The No.1 BF in the west district of Handan Iron and Steel Co., Ltd. was not active for a long time with wet coke oven hearth, and the iron tapping was not smooth after the field dumping in front of the furnace. In this paper, the causes of furnace temperature cooling and the countermeasures are summarized. By optimizing the tapping scheme and reasonably controlling the operation parameters, the normal production level can be quickly restored and good results have been achieved.

关 键 词:高炉 炉温大凉 炉况恢复 

分 类 号:TF548[冶金工程—钢铁冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象