Influence of Fe Content on Tool Galling in Ironing Aluminum Beverage Cans  

Influence of Fe Content on Tool Galling in Ironing Aluminum Beverage Cans

在线阅读下载全文

作  者:Aleksey Vladimirovich Andrianov Elena Gennadievna Kandalova Evgeniy Vladimirovich Aryshensky 

机构地区:[1]FRP Heat Treatment Department, ZAO “Alcoa SMZ”, Samara, Russia [2]Industrial Engineering Department, Samara State Aerospace University, Samara, Russia [3]Technological Development Department, ZAO “Alcoa SMZ”, Samara, Russia

出  处:《Materials Sciences and Applications》2014年第10期719-723,共5页材料科学与应用期刊(英文)

摘  要:Insoluble constituents in 3104 alloy for beverage cans manufacturing play an important role in deep ironing process. This paper studies the effect of Fe content in the alloy on volume fraction of the constituents Al6(Fe, Mn)3 and Al12(Fe, Mn)3Si and its influence on ironing die pickup. It is shown that with Fe content increase, the amount of these constituents rises that helps prevent tool galling. Trials made at a can plant showed less ironing die changeovers at bodymakers. The optimum Fe content for aluminum can production can be considered between 0.47% and 0.53% that corresponds to 2.0% - 2.3% of insoluble constituent volume fraction. Greater amounts than this cause problems with excessive constituent particle formation and earing;smaller amounts result in increased ironing die galling.Insoluble constituents in 3104 alloy for beverage cans manufacturing play an important role in deep ironing process. This paper studies the effect of Fe content in the alloy on volume fraction of the constituents Al6(Fe, Mn)3 and Al12(Fe, Mn)3Si and its influence on ironing die pickup. It is shown that with Fe content increase, the amount of these constituents rises that helps prevent tool galling. Trials made at a can plant showed less ironing die changeovers at bodymakers. The optimum Fe content for aluminum can production can be considered between 0.47% and 0.53% that corresponds to 2.0% - 2.3% of insoluble constituent volume fraction. Greater amounts than this cause problems with excessive constituent particle formation and earing;smaller amounts result in increased ironing die galling.

关 键 词:3104 Alloy IRONING ALUMINUM TOOL GALLING FE CONTENT Insoluble Constituents 

分 类 号:R73[医药卫生—肿瘤]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象