The present work attributes the role of boron on the high strength steel submerged arc weld using an undermatching filler wire.Mild steel filler wire was used for welding in constant machine parameters setting to eval...
This work was supported by the China Postdoctoral Science Foundation C Grant No. 2014M550414 ) and the National Natural Science Foundation of China ( Grant No. 51401152).
In this study, the effects of Zr-Ti combined deoxidation and AI deoxidation on the impact toughness of coarse- grained heat-affected zone in high-strength low-alloy steels were investigated. More fine oxides were form...
9Cr-1Mo ferritic steels have been used in the conventional power generation plants due to their excellent creep resistance. However, one of the main obstacles in welding 9Cr-1Mo steels is the formation of undesirable ...
Based on welding thermal simulation on Nb-microaUoyed XSO pipeline stee! using Gleeble-3500 thermal simulation equipment, microstlttcture and impact toughness in coarse grain heat-affected zone (CGHAZ) under differe...
The microstractures of 9Cr-lMo multipass deposited metal were observed. The effect of microstructure on impact toughness of 9Cr-lMo multipass deposited metal with varying heat inputs was investigated. Result shows tha...
Effects of CeF3 on properties of self-shielded flux cored wire including welding process, inclusions in weld metal and mechanical properties are systematically studied. Welding smoke and spatter are reduced with the a...
Charpy impact test and COD test were performed on the specimens subjected to simulated welded thermal cycle and the specimens taken from welded joint. The optical microscope, TEM, SEM, EDAX and XRD analysis have been ...
The effect of Al in Ti-microalloyed welding wire on microstructure and toughness of deposited metals is studied.The results show that the deposited metal toughness worsens with increasing Al in wire' The mechanism of...
By using thermo-simulation,Auger analysis and Charpy Ⅴ impact test and with the observation of the microstructures in which cleavage crack was initiated,the morphology and toughness of the local brittle zone of C-Mn ...