supported by the National Natural Science Foundation of China(51672220,51902258,51972265);Fundamental Research Funds for the Central Universities(3102019GHXM002);State Key Laboratory of Solidification Processing Project(2019-TZ-04)of China,China Postdoctoral Science Foundation(2019M653729);Natural Science Foundation of Shaanxi Province(2019JQ-621);the Shaanxi Province Postdoctoral Science Foundation(2017BSHEDZZ07).
(1-x)(0.8Bi_(1/2)Na_(1/2)TiO3-0.2Bi_(1/2)K_(1/2)TiO3)-xBi(Ni_(2/3)Nb_(1/3))O3(BNKT-xBNN)solid solution ceramics were fabricated by high temperature solid-state reaction method.All the compositions possess relaxor ferr...
Funded by the National Natural Science Foundation of China(No.51302093);the Fundamental Research Funds for the Central Universities of China(Nos.2014TS046,2015MS017)
(Ba(0.6) Sr(0.4))(0.85) Bi(0.1) TiO3 ceramics doped with x wt%CaZrO3(x= 0-10) were synthesized by solid-state reaction method. The effects of CaZrO3 amount on the dielectric properties and structure of(Ba...