Project(2006AA03Z413) supported by the Hi-tech Research and Development Program of China
SnO2 nanoparticles with the average particle size of 5-30 nm were synthesized using SnCl4·5H2O as the precursor and NH3·H2O as the mineralizing agent by hydrothermal method.In the case of 1 kg/batch production,the e...