试验了830~910℃固溶处理和480~540℃时效对Φ20 mm NAK80塑料模具钢(/%:0.15C,0.30Si,1.50Mn,3.00Ni,1.00Cu,1.00Al,0.30Mo,0.30Cr)组织和硬度的影响,并对其时效动力学行为进行了研究。结果表明,890℃固溶处理后,NAK80钢组织由板条马...
China Ministry of Science and Technology under Contract (2010CB631203);National Natural Science Foundation of China (51001021);Doctoral Fund of Ministry of Education of China (20100042120008, 20100042110006)