A surface Ti-WC composite was fabricated on CP-Ti by surface friction stirring(SFS)using a pinless WC-Cotool at a processing window of 800−2500 r/min and 8−50 mm/min.At 1600 r/min-50 mm/min,a defect-free compositelaye...
financial support from the National Natural Science Foundation of China(22078326,21878305).
In this study,the effects of reaction parameters on the deep-reduction and carbonization process of WO_(2)-Co to WC-Co were studied.The results indicate that the oxygen loss rate of WO_(2) is positively correlated wit...